<div dir="ltr"><div>Hi,</div><div><br></div><div>We have recently ordered a few grids from Quantifoil with R 3/3 on Cu 300 mesh grids + 3 nm C  (Holey Carbon Films with ~ 3 nm continuous carbon on top) configuration. </div><div><br></div><div>I have been observing recently that many of the grids of the batch have no carbon in the hole when we screen them after sample freezing. Now, I am wondering if it is possible/common that this problem can arise?</div><div><br></div><div>Otherwise, I would be more skeptical about our freezing or extended glow discharge!</div><div><br></div><div>Thanks!</div></div>